高 γ′相含量GH4151变形高温合金铸态组织与开裂敏感性分析
钟佳, 王法, 江河, 姚志浩, 董建新

Analyses of As-Cast Microstructure and Cracking Sensitivity of GH4151 Wrought Superalloy with High γ′ Phase Content
ZHONG Jia, WANG Fa, JIANG He, YAO Zhihao, DONG Jianxin
图5 GH4151合金萃取析出相粉末的XRD谱
Fig.5 XRD spectra of precipitated phase powders extracted from GH4151 alloy
(a) γ' phase (b) MC carbides, Laves phase, and η phase