高 γ′相含量GH4151变形高温合金铸态组织与开裂敏感性分析 |
| 钟佳, 王法, 江河, 姚志浩, 董建新 |
|
Analyses of As-Cast Microstructure and Cracking Sensitivity of GH4151 Wrought Superalloy with High γ′ Phase Content |
| ZHONG Jia, WANG Fa, JIANG He, YAO Zhihao, DONG Jianxin |
| 图1 直径410 mm的GH4151合金自耗锭不同区域枝晶形貌的OM像 |
| Fig.1 OM images showing the dendritic morphologies in different regions of GH4151 alloy consumable ingot with a diameter of 410 mm (a) edge region (b) 1/2 radius region (c) center region |
|