固溶后处理对GH4706合金时效析出相演化及力学性能的影响
王冲, 王磊, 段然, 田强, 黄烁, 赵光普

Effects of Solution Post-Treatment on Precipitation Evolution During Aging of GH4706 Alloy and Its Mechanical Properties
WANG Chong, WANG Lei, DUAN Ran, TIAN Qiang, HUANG Shuo, ZHAO Guangpu
表3 不同固溶后处理和双级时效后GH4706合金冲击吸收功各组成对比 (J)
Table 3 Comparisons of the impact absorption energy components of GH4706 alloy after different solution post-treatments and the two-stage aging treatment

Solution

post-treatment

EeEpEc
AA5.9518.5752.26
FSA6.915.6914.68
FA6.1414.4435.59
FAs6.3917.7933.77