固溶后处理对GH4706合金时效析出相演化及力学性能的影响 |
| 王冲, 王磊, 段然, 田强, 黄烁, 赵光普 |
|
Effects of Solution Post-Treatment on Precipitation Evolution During Aging of GH4706 Alloy and Its Mechanical Properties |
| WANG Chong, WANG Lei, DUAN Ran, TIAN Qiang, HUANG Shuo, ZHAO Guangpu |
| 图12 不同固溶后处理和双级时效后GH4706合金室温冲击试样断口纵截面组织的局部取向差(KAM)图和SEM像 |
| Fig.12 Kernel average misorientation (KAM) maps (a, c, e, g) and SEM images (b, d, f, h) showing the fracture morphologies of longitudinal sections of the impact test samples at room temperature after AA (a, b), FSA (c, d), FA (e, f), and FAs (g, h) solution post-treatments and the two-stage aging treatment (Red arrows in Figs.12b, d, f, and h show the (Nb, Ti)C, and blue arrows in Figs.12d, f, and h show the cellular microstructures. Inset images in Figs.12d, f, and h show the locally enlarged views, inset curve in Fig.12d shows the EDS result of (Nb, Ti)C) |
|