固溶后处理对GH4706合金时效析出相演化及力学性能的影响
王冲, 王磊, 段然, 田强, 黄烁, 赵光普

Effects of Solution Post-Treatment on Precipitation Evolution During Aging of GH4706 Alloy and Its Mechanical Properties
WANG Chong, WANG Lei, DUAN Ran, TIAN Qiang, HUANG Shuo, ZHAO Guangpu
图11 JMatPro模拟计算和不同固溶后处理实测的连续冷却转变(CCT)图
Fig.11 Continuous-cooling-transformation (CCT) diagrams of JMatPro simulation (a) and the actual solution post-treatments (b) (Inset in Fig.11b shows the locally enlarged diagram)