固溶后处理对GH4706合金时效析出相演化及力学性能的影响
王冲, 王磊, 段然, 田强, 黄烁, 赵光普

Effects of Solution Post-Treatment on Precipitation Evolution During Aging of GH4706 Alloy and Its Mechanical Properties
WANG Chong, WANG Lei, DUAN Ran, TIAN Qiang, HUANG Shuo, ZHAO Guangpu
图1 GH4706涡轮盘取样位置示意图
Fig.1 Schematic of sample cutting position in the GH4706 turbine disc (R—radius)