坯体成形工艺对烧结制备超细晶WC-12Co硬质合金组织和力学性能的影响 |
| 王超, 王海滨, 玄拾雷, 刘轩, 刘雪梅, 宋晓艳 |
|
Effects of Powder Molding Process on the Microstructure and Mechanical Properties of As-Sintered Ultrafine- Grained WC-12Co Cemented Carbides |
| WANG Chao, WANG Haibin, XUAN Shilei, LIU Xuan, LIU Xuemei, SONG Xiaoyan |
| 图10 PEG质量分数为1.5%及PEG浓度为4.1%时坯体密度对烧结制备WC-12Co硬质合金力学性能的影响 |
| Fig.10 Effects of green density on mechanical properties of the sintered WC-12Co cemented carbides under PEG content of 1.5% and PEG solution concentration of 4.1% |
|