纳米压痕下VCoNi 中熵合金的塑性变形行为
王方圆, 张玉龙, 王章维, 熊志平, 王辉, 宋旼, 夏文真

Plastic Deformation Behaviors of VCoNi Medium-Entropy Alloy Under Nanoindentation
WANG Fangyuan, ZHANG Yulong, WANG Zhangwei, XIONG Zhiping, WANG Hui, SONG Min, XIA Wenzhen
图5 5 mN压痕载荷下各晶粒滑移台阶的局部放大SE像和相应滑移面示意图
Fig.5 Partially enlarged SE images of slip steps and schematics of slip planes (insets) of {101} grain in Fig.3a (a, b), {111} grain in Fig.3d (c, d), and {001}grain in Fig.3g (e, f) (Red arrows in boxes indicate the direction of dislocation movement; 1-6 represent the junctions of dislocation interactions)