纳米压痕下VCoNi 中熵合金的塑性变形行为 |
| 王方圆, 张玉龙, 王章维, 熊志平, 王辉, 宋旼, 夏文真 |
|
Plastic Deformation Behaviors of VCoNi Medium-Entropy Alloy Under Nanoindentation |
| WANG Fangyuan, ZHANG Yulong, WANG Zhangwei, XIONG Zhiping, WANG Hui, SONG Min, XIA Wenzhen |
| 图2 80 mN压痕载荷下滑移台阶局部放大SE像 |
| Fig.2 Partially enlarged SE images of slip steps in {101} grain (a) and {001} grain (b, c) under 80 mN indentation load (Dotted rectangles represent the slip steps formed by dislocations sliding along the slip plane before double cross-slip, solid rectangles represent the slip steps formed by dislocations sliding along the slip plane after double cross-slip. (a) box 1 in Fig.1a (b) box 2 in Fig.1c (c) box 3 in Fig.1c |
|