TC18钛合金大尺寸 β 晶粒制备及典型织构对力学性能的影响
颜孟奇, 吴泽浩, 佟健博, 黄利军, 黄驿胜

Preparation of Large-Sized β Grains and Effect of Typical Textures on Mechanical Properties of TC18 Titanium Alloy
YAN Mengqi, WU Zehao, TONG Jianbo, HUANG Lijun, HUANG Yisheng
图3 TC18钛合金低倍片中显微组织观测试样的取样位置示意图
Fig.3 Schematic of sampling position for microstructure observation specimens in TC18 titanium alloy for macrostructure test