TC18钛合金大尺寸 β 晶粒制备及典型织构对力学性能的影响 |
| 颜孟奇, 吴泽浩, 佟健博, 黄利军, 黄驿胜 |
|
Preparation of Large-Sized β Grains and Effect of Typical Textures on Mechanical Properties of TC18 Titanium Alloy |
| YAN Mengqi, WU Zehao, TONG Jianbo, HUANG Lijun, HUANG Yisheng |
| 图2 TC18钛合金坯料力学性能测试试样的取样位置示意图及试样尺寸图 |
| Fig.2 Schematics of sampling position (a) and dimensions of tensile (b) and impact (c) specimens for TC18 titanium alloy billet (unit: mm) |
|