TC18钛合金大尺寸 β 晶粒制备及典型织构对力学性能的影响 |
| 颜孟奇, 吴泽浩, 佟健博, 黄利军, 黄驿胜 |
|
Preparation of Large-Sized β Grains and Effect of Typical Textures on Mechanical Properties of TC18 Titanium Alloy |
| YAN Mengqi, WU Zehao, TONG Jianbo, HUANG Lijun, HUANG Yisheng |
| 图1 TC18钛合金坯料锻造工艺示意图 |
| Fig.1 Schematics of forging process for TC18 titanium alloy billets (LD—length direction, TD1—transverse direction 1, TD2—transverse direction 2) (a) forging at α + β region (b) forging at β region |
|