热处理对电弧定向能量沉积Al-Zn-Mg-Cu-Sc合金显微组织与力学性能的影响
秦凤明, 李亚菲, 李亚杰, 赵晓东, 梁上上, 陈金秋

Effect of Heat Treatment on the Microstructural Characteristics and Mechanical Properties of Al-Zn-Mg-Cu-Sc Alloy Prepared via Wire-Arc Directed Energy Deposition Process
QIN Fengming, LI Yafei, LI Yajie, ZHAO Xiaodong, LIANG Shangshang, CHEN Jinqiu
表1 材料的化学成分 (mass fraction / %)
Table 1 Chemical compositions of the materials
AlloyZnMgCuScCrFeSiTiAl
7075-Sc wire5.522.561.620.250.110.320.250.14Bal.