热处理对电弧定向能量沉积Al-Zn-Mg-Cu-Sc合金显微组织与力学性能的影响 |
| 秦凤明, 李亚菲, 李亚杰, 赵晓东, 梁上上, 陈金秋 |
|
Effect of Heat Treatment on the Microstructural Characteristics and Mechanical Properties of Al-Zn-Mg-Cu-Sc Alloy Prepared via Wire-Arc Directed Energy Deposition Process |
| QIN Fengming, LI Yafei, LI Yajie, ZHAO Xiaodong, LIANG Shangshang, CHEN Jinqiu |
| 图3 沉积态与时效态电弧DED合金的EBSD反极图、极图和晶粒尺寸统计图 |
| Fig.3 EBSD inverse pole figures (a1-d1), pole figures (a2-d2), and grain size statistics (a3-d3) of the wire-arc DED alloys under the as-deposited state (a1-a3) and as-aged at 470 oC, 4 h + 120 oC, 12 h (b1-b3), 470 oC, 4 h + 120 oC, 18 h (c1-c3), and 470 oC, 4 h + 120 oC, 24 h (d1-d3) |
|