低合金高强钢板贝/马复相回火过程硬度及微观组织的演变行为 |
| 鞠玉琳, 魏琪, 袁志钟, 程晓农 |
|
Hardness and Microstructural Evolution of Lower Bainite and Martensite Mixtures on Tempering of High-Strength Low-Alloy Steel Plates |
| JU Yulin, WEI Qi, YUAN Zhizhong, CHENG Xiaonong |
| 图9 600 ℃回火100 h后,LB/M (56%M + 44%LB)和100%LB试样中板条尺寸分布,以及100%M、LB/M (56%M + 44%LB)和100%LB试样中碳化物宽度和长度尺寸分布 |
| Fig.9 Lath size distribution for the 100% LB and LB/M (56%M + 44%LB) samples (a), and the carbide width (b) and length (c) distributions for the 100%M, LB/M (56%M + 44%LB), and 100%LB samples after tempering at 600 oC for 100 h |
|