热处理工艺对选区激光熔化成型18Ni300马氏体时效钢微观组织及力学性能的影响 |
| 吴文伟, 向超, 张涛, 邹志航, 孙勇飞, 刘金鹏, 张涛, 韩恩厚 |
|
Effect of Heat Treatment on Microstructure and Mechanical Properties of 18Ni300 Maraging Steel Fabricated by Selective Laser Melting |
| WU Wenwei, XIANG Chao, ZHANG Tao, ZOU Zhihang, SUN Yongfei, LIU Jinpeng, ZHANG Tao, HAN En-Hou |
| 图16 不同热处理状态SLM 18Ni300试样屈服强度的理论值和测试值 |
| Fig.16 Estimated and experimental results of yield strength of SLM 18Ni300 samples after heat treatments (ΔσMart—phase transformation streng-thening, Δσss—solid solution strengthening, Δσp—precipitation strengthening) |
|