基于轧制温度调控的Fe50Mn29Co10Cr10Cu1 高熵合金微观组织与力学性能
王家骏, 袁野, 何竹风, 朱明伟, 贾楠

Microstructures and Mechanical Properties of the Fe50Mn29Co10Cr10Cu1 High-Entropy Alloy Regulated by Rolling Temperature
WANG Jiajun, YUAN Ye, HE Zhufeng, ZHU Mingwei, JIA Nan
图7 不同工艺制备的样品工程应力-应变曲线、真应力-应变曲线和应变硬化率曲线
Fig.7 Engineering stress-strain curves (a), true stress-strain curves (b), and strain hardening rate curves (c) of the samples prepared by different processing routes