基于轧制温度调控的Fe50Mn29Co10Cr10Cu1 高熵合金微观组织与力学性能 |
| 王家骏, 袁野, 何竹风, 朱明伟, 贾楠 |
|
Microstructures and Mechanical Properties of the Fe50Mn29Co10Cr10Cu1 High-Entropy Alloy Regulated by Rolling Temperature |
| WANG Jiajun, YUAN Ye, HE Zhufeng, ZHU Mingwei, JIA Nan |
| 图4 LNR40% + AN500 ℃样品的TEM像及选区电子衍射(SAED)花样 |
| Fig.4 TEM images and the selected area electron diffraction (SAED) patterns (insets) of the LNR40% + AN500 oC sample showing deformation twins (a), twin intersection (b), microbands (c), and dislocation cells (d) (T—twin, BF—bright field, DF—dark field) |
|