基于轧制温度调控的Fe50Mn29Co10Cr10Cu1 高熵合金微观组织与力学性能
王家骏, 袁野, 何竹风, 朱明伟, 贾楠

Microstructures and Mechanical Properties of the Fe50Mn29Co10Cr10Cu1 High-Entropy Alloy Regulated by Rolling Temperature
WANG Jiajun, YUAN Ye, HE Zhufeng, ZHU Mingwei, JIA Nan
图2 经不同工艺制备的样品的SEM像及晶粒尺寸分布图
Fig.2 SEM images (a-f) and grain size distribution maps (g-i) of the samples prepared by different processing routes (d—average grain size, RD—rolling direction, ND—normal direction )
(a) LNR40% + AN500 oC (b) CR40% + AN500 oC (c) WR40% + AN500 oC (d, g) LNR40% + AN800 oC (e, h) CR40% + AN800 oC (f, i) WR40% + AN800 oC