基于轧制温度调控的Fe50Mn29Co10Cr10Cu1 高熵合金微观组织与力学性能 |
| 王家骏, 袁野, 何竹风, 朱明伟, 贾楠 |
|
Microstructures and Mechanical Properties of the Fe50Mn29Co10Cr10Cu1 High-Entropy Alloy Regulated by Rolling Temperature |
| WANG Jiajun, YUAN Ye, HE Zhufeng, ZHU Mingwei, JIA Nan |
| 图1 经轧制结合退火制备的样品拉伸前后的XRD谱 |
| Fig.1 XRD spectra of samples prepared by rolling and annealing before (a) and after (b) tensile tests (LNR—liquid nitrogen rolling, CR—cold rolling at room temperature, WR—warm rolling, AN—annealing) |
|