冷喷涂后处理技术及其研究进展 |
| 刘瑞良, 刘泉利, 李富霖 |
|
Post-Treatment Technologies of Cold Spray and Their Research Advance |
| LIU Ruiliang, LIU Quanli, LI Fulin |
| 图7 采用冷喷涂和热轧工艺制备Mg/Al复合板材流程图[ |
| Fig.7 Flow charts of Mg/Al composite plate prepared by cold spraying and hot rolling[ |
|