冷喷涂后处理技术及其研究进展
刘瑞良, 刘泉利, 李富霖

Post-Treatment Technologies of Cold Spray and Their Research Advance
LIU Ruiliang, LIU Quanli, LI Fulin
图3 不同温度、时间热处理后冷喷涂316L不锈钢涂层的微观组织演变[48]
Fig.3 Microstructure evolutions of cold spray 316L stainless steel coatings after heat treatment at different temperatures and time[48]