冷喷涂后处理技术及其研究进展 |
| 刘瑞良, 刘泉利, 李富霖 |
|
Post-Treatment Technologies of Cold Spray and Their Research Advance |
| LIU Ruiliang, LIU Quanli, LI Fulin |
| 图2 高温热处理过程中冷喷涂涂层中变形Ti6Al4V颗粒的显微组织演变[ |
| Fig.2 Schematics of microstructure evolution of deformed Ti6Al4V particles in cold spray (CS) deposition coating during high temperature heat treatment (HT) (IPB—inter-particle bonding)[ (b1) grains in as-sprayed copper coating (b2) uniformly grown grains after optimal annealing (b3) abnormally grown grains over optimal annealing temperature |
|