过冷(Fe1 -x Co x)79.3B20.7 合金的凝固 |
| 杨林, 马长松, 刘连杰, 李金富 |
|
Solidification of Undercooled (Fe1 -x Co x)79.3B20.7 Alloys |
| YANG Lin, MA Changsong, LIU Lianjie, LI Jinfu |
| 图10 各成分合金的凝固路径示意图 |
| Fig.10 Schematic of solidification paths for various alloys under different undercoolings |
|