过冷(Fe1 -x Co x)79.3B20.7 合金的凝固 |
| 杨林, 马长松, 刘连杰, 李金富 |
|
Solidification of Undercooled (Fe1 -x Co x)79.3B20.7 Alloys |
| YANG Lin, MA Changsong, LIU Lianjie, LI Jinfu |
| 图7 (Fe0.2Co0.8)79.3B20.7合金的凝固冷却曲线、XRD谱及不同过冷度下合金组织的OM像和EBSD像 |