过冷(Fe1 -x Co x)79.3B20.7 合金的凝固 |
| 杨林, 马长松, 刘连杰, 李金富 |
|
Solidification of Undercooled (Fe1 -x Co x)79.3B20.7 Alloys |
| YANG Lin, MA Changsong, LIU Lianjie, LI Jinfu |
| 图4 (Fe0.6Co0.4)79.3B20.7合金的凝固冷却曲线、XRD谱及不同过冷度下合金组织的OM像 |
| Fig.4 Cooling curves (a), XRD spectra (b), and OM images (c-f) of (Fe0.6Co0.4)79.3B20.7 alloy under different undercoolings (Insets in Figs.4c-f are magnified views of the areas indicated by the white rectangles) (c) ΔT = 44 K (d) ΔT = 162 K (e) ΔT = 326 K (f) ΔT = 369 K |
|