过冷(Fe1 -x Co x)79.3B20.7 合金的凝固
杨林, 马长松, 刘连杰, 李金富

Solidification of Undercooled (Fe1 -x Co x)79.3B20.7 Alloys
YANG Lin, MA Changsong, LIU Lianjie, LI Jinfu
图3 (Fe0.8Co0.2)79.3B20.7合金的凝固冷却曲线、XRD谱及不同过冷度(ΔT)下合金组织的OM像
Fig.3 Cooling curves (a), XRD spectra (b), and OM images (c-f) of (Fe0.8Co0.2)79.3B20.7 alloy under different undercoolings (ΔT) (Insets in Figs.3d-f show the higher magnification microstructures, TL is the liquidus temperature of the alloy, TE, α‐M/M2B is the temperature of the eutectic reaction L→α-M + M2B, and TL,M23B6 is the melting temperature of M23B6 phase)
(c) ΔT = 10 K (d) ΔT = 233 K (e) ΔT = 305 K (f) ΔT = 351 K