过冷(Fe1 -x Co x)79.3B20.7 合金的凝固 |
| 杨林, 马长松, 刘连杰, 李金富 |
|
Solidification of Undercooled (Fe1 -x Co x)79.3B20.7 Alloys |
| YANG Lin, MA Changsong, LIU Lianjie, LI Jinfu |
| 图2 (Fe1 - x Co x)79.3B20.7母合金锭组织的OM像 |
| Fig.2 OM images of (Fe1 - x Co x)79.3B20.7 alloy ingots (Inset in Fig.2d shows the higher magnification microstructure) (a) x = 0 (b) x = 0.2 (c) x = 0.4 (d) x = 0.6 (e) x = 0.8 (f) x = 1.0 |
|