CrNbTiVAl x 难熔高熵合金的组织、力学性能和高温氧化行为
|
|
朱满, 张成, 许军锋, 坚增运, 惠增哲
|
Microstructure, Mechanical Properties, and High-Temperature Oxidation Behaviors of the CrNbTiVAl x Refractory High-Entropy Alloys
|
|
ZHU Man, ZHANG Cheng, XU Junfeng, JIAN Zengyun, XI Zengzhe
|
|
表1 CrNbTiVAl x 难熔高熵合金不同区域的EDS结果 (atomic fraciton / %)
|
Table 1 EDS results in different regions of the CrNbTiVAl x RHEAs
|
|
| Alloy | Region | Cr | Nb | Ti | V | Al |
|---|
| Al0.25 | Nominal | 23.53 | 23.53 | 23.53 | 23.53 | 5.88 | | bcc | 27.32 | 27.24 | 10.55 | 29.00 | 5.89 | | Laves | 30.97 | 25.19 | 11.33 | 25.96 | 6.54 | | α-Ti | 00.23 | 05.40 | 90.29 | 03.96 | 0.12 | | Al0.50 | Nominal | 22.22 | 22.22 | 22.22 | 22.22 | 11.12 | | bcc | 33.29 | 22.58 | 16.14 | 18.76 | 09.23 | | Laves | 33.41 | 23.64 | 14.50 | 19.62 | 08.84 | | α-Ti | 00.45 | 04.67 | 90.96 | 03.48 | 00.13 | | Al0.75 | Nominal | 21.05 | 21.05 | 21.05 | 21.05 | 15.80 | | bcc | 21.22 | 22.99 | 17.40 | 23.48 | 14.91 | | Laves | 30.44 | 20.28 | 16.65 | 22.02 | 10.62 | | α-Ti | 00.45 | 05.39 | 89.30 | 04.53 | 00.34 | | Al1.0 | Nominal | 20 | 20 | 20 | 20 | 20 | | bcc | 20.52 | 19.62 | 19.84 | 20.08 | 19.06 | | Laves | 31.27 | 18.33 | 17.63 | 20.38 | 12.39 | | α-Ti | 00.11 | 03.46 | 93.10 | 03.04 | 00.29 |
|
|
|