CrNbTiVAl x 难熔高熵合金的组织、力学性能和高温氧化行为 |
| 朱满, 张成, 许军锋, 坚增运, 惠增哲 |
|
Microstructure, Mechanical Properties, and High-Temperature Oxidation Behaviors of the CrNbTiVAl x Refractory High-Entropy Alloys |
| ZHU Man, ZHANG Cheng, XU Junfeng, JIAN Zengyun, XI Zengzhe |
| 图7 CrNbTiVAl x 难熔高熵合金900 ℃氧化100 h后的表面形貌 |
| Fig.7 Low (a-d) and high (e-h) magnified surface morphologies of the CrNbTiVAl x RHEAs after oxidation at 900 oC for 100 h (a, e) Al0.25 (b, f) Al0.5 (c, g) Al0.75 (d, h) Al1.0 |
|