CrNbTiVAl x 难熔高熵合金的组织、力学性能和高温氧化行为 |
| 朱满, 张成, 许军锋, 坚增运, 惠增哲 |
|
Microstructure, Mechanical Properties, and High-Temperature Oxidation Behaviors of the CrNbTiVAl x Refractory High-Entropy Alloys |
| ZHU Man, ZHANG Cheng, XU Junfeng, JIAN Zengyun, XI Zengzhe |
| 图2 CrNbTiVAl x 难熔高熵合金微观组织的背散射电子(BSE)像 |
| Fig.2 Backscattered electron (BSE) images of microstructures of the CrNbTiVAl x RHEAs (a) Al0.25 (b) Al0.5 (c) Al0.75 (d) Al1.0 |
|