激光熔覆难熔高熵合金涂层研究进展 |
| 夏兴川, 张恩宽, 丁俭, 王玉江, 刘永长 |
|
Research Progress on Laser Cladding of Refractory High-Entropy Alloy Coatings |
| XIA Xingchuan, ZHANG Enkuan, DING Jian, WANG Yujiang, LIU Yongchang |
| 图2 激光熔覆(LC)和磁场-LC制备的MoNbTaW难熔高熵合金涂层(RHEACs)截面形貌以及局部区域放大的显微形貌[ |
| Fig.2 SEM images of cross-section and enlarged images of MoNbTaW refractory high entropy alloy coatings (RHEACs) prepared by laser cladding (LC) without (a1-d1) and with (a2-d2) magnetic field[ |
|