表3 快速凝固和锻造态Allvac 718Plus合金在704和760 ℃长期时效的γ′相粗化速率[29] (nm3·h-1)
Table 3 Coarsening rates of γ′ phase of the rapidly-solidified and forged Allvac 718Plus alloy at 704 and 760 oC[29]
State of Allvac 718Plus alloy704 oC760 oC
Rapidly-solidified14.483.2
Forged08.764.4