Allvac 718Plus高温合金第二相演变与性能研究进展 |
| 唐丽婷, 郭倩颖, 李冲, 丁然, 刘永长 |
|
Advances in Secondary Phase Evolution and Performance Enhancement of Allvac 718Plus Superalloy |
| TANG Liting, GUO Qianying, LI Chong, DING Ran, LIU Yongchang |
| 图9 经固溶处理后炉冷至时效温度的锻造态Allvac 718Plus在长期时效过程中γ″/γ′复合结构的演变示意图[ |
| Fig.9 A qualitative model schematic illustration directly showing the evolution of γ″/γ′ coprecipitates[ (a) all evolution process in forged Allvac 718Plus alloy during long-term thermal exposures at 705 oC (b) the evolution from γ′ to sandwich-γ″/γ′/γ″ coprecipitates (c) the evolution from sandwich-γ″/γ′/γ″ coprecipitates to partly compact-γ″/γ′ coprecipitates (d) the evolution from sandwich-γ″/γ′/γ″ coprecipitates and partly compact-γ″/γ′ coprecipitates to all compact-γ″/γ′/γ″ coprecipitates |
|