Ni43.5Co19Cr10Fe10Al15Ti2Mo0.5 共晶高熵合金快速凝固行为及组织调控 |
| 卢健麟, 任化永, 谢桉, 王建潼, 何峰 |
|
Rapid Solidification Behavior and Microstructure Regulation of Ni43.5Co19Cr10Fe10Al15Ti2Mo0.5 Eutectic High-Entropy Alloy |
| LU Jianlin, REN Huayong, XIE An, WANG Jiantong, HE Feng |
| 图6 打印态SLM-C试样垂直于增材方向截面的TEM像、选区电子衍射(SAED)花样及EDS分析 |
| Fig.6 TEM images (a, f), selected area electron diffraction (SAED) patterns (b-d), and EDS analyses (e, g, h) of the as-print SLM-C specimen along the cross-section perpendicular to the additive direction (d) Kurdjumov-Sachs (K-S) relation between B2 and fcc phases (e) EDS line scanning result (g, h) EDS mappings of Al (g) and Ti (h) |
|