Ni43.5Co19Cr10Fe10Al15Ti2Mo0.5 共晶高熵合金快速凝固行为及组织调控 |
| 卢健麟, 任化永, 谢桉, 王建潼, 何峰 |
|
Rapid Solidification Behavior and Microstructure Regulation of Ni43.5Co19Cr10Fe10Al15Ti2Mo0.5 Eutectic High-Entropy Alloy |
| LU Jianlin, REN Huayong, XIE An, WANG Jiantong, HE Feng |
| 图3 铸态试样各个区域的SEM像及EDS分析 |
| Fig.3 SEM images (a, d, g) and EDS analyses (b, c, e, f, h, i) of different crystal zones of the as-cast specimen (Arrows in Fig.3a, b, d, e, g, and h show the EDS line scanming directions) (a, b, c) chill crystal zones (d, e, f) columnar zones (g, h, i) equiaxed grain zones |
|