Ni43.5Co19Cr10Fe10Al15Ti2Mo0.5 共晶高熵合金快速凝固行为及组织调控 |
| 卢健麟, 任化永, 谢桉, 王建潼, 何峰 |
|
Rapid Solidification Behavior and Microstructure Regulation of Ni43.5Co19Cr10Fe10Al15Ti2Mo0.5 Eutectic High-Entropy Alloy |
| LU Jianlin, REN Huayong, XIE An, WANG Jiantong, HE Feng |
| 图2 铸态试样截面不同区域的OM像及EBSD像 |