预时效处理对冷轧含Al奥氏体耐热钢组织和性能的影响 |
| 张胜煜, 马庆爽, 余黎明, 张竟文, 李会军, 高秋志 |
|
Effect of Pre-Aging on Microstructure and Properties of Cold-Rolled Alumina-Forming Austenitic Steel |
| ZHANG Shengyu, MA Qingshuang, YU Liming, ZHANG Jingwen, LI Huijun, GAO Qiuzhi |
| 图16 4Al-2Cu-AFA钢微观组织演变示意图 |
| Fig.16 Schematic of microstructural evolution of 4Al-2Cu-AFA steel |
|