预时效处理对冷轧含Al奥氏体耐热钢组织和性能的影响 |
| 张胜煜, 马庆爽, 余黎明, 张竟文, 李会军, 高秋志 |
|
Effect of Pre-Aging on Microstructure and Properties of Cold-Rolled Alumina-Forming Austenitic Steel |
| ZHANG Shengyu, MA Qingshuang, YU Liming, ZHANG Jingwen, LI Huijun, GAO Qiuzhi |
| 图13 CR10-A100试样和PA24-CR10-A100试样中析出相的尺寸统计 |
| Fig.13 Statistics on the size of B2-NiAl precipitates (a, b) and Laves precipitates (c, d) in CR10-A100 (a, c) and PA24-CR10-A100 (b, d) samples |
|