预时效处理对冷轧含Al奥氏体耐热钢组织和性能的影响 |
| 张胜煜, 马庆爽, 余黎明, 张竟文, 李会军, 高秋志 |
|
Effect of Pre-Aging on Microstructure and Properties of Cold-Rolled Alumina-Forming Austenitic Steel |
| ZHANG Shengyu, MA Qingshuang, YU Liming, ZHANG Jingwen, LI Huijun, GAO Qiuzhi |
| 图8 CR10试样和PA24-CR10试样700 ℃时效处理不同时间后Vickers硬度的变化 |
| Fig.8 Variations in Vickers hardness of CR10 and PA24-CR10 samples aged at 700 oC for different time |
|