预时效处理对冷轧含Al奥氏体耐热钢组织和性能的影响 |
| 张胜煜, 马庆爽, 余黎明, 张竟文, 李会军, 高秋志 |
|
Effect of Pre-Aging on Microstructure and Properties of Cold-Rolled Alumina-Forming Austenitic Steel |
| ZHANG Shengyu, MA Qingshuang, YU Liming, ZHANG Jingwen, LI Huijun, GAO Qiuzhi |
| 图6 PA24-CR10-A500试样中δ-铁素体区的SEM像及相应的EDS面扫描结果 |
| Fig.6 SEM image and corresponding EDS mapping results of the δ-ferritic region in the PA24-CR10-A500 sample |
|