预时效处理对冷轧含Al奥氏体耐热钢组织和性能的影响 |
| 张胜煜, 马庆爽, 余黎明, 张竟文, 李会军, 高秋志 |
|
Effect of Pre-Aging on Microstructure and Properties of Cold-Rolled Alumina-Forming Austenitic Steel |
| ZHANG Shengyu, MA Qingshuang, YU Liming, ZHANG Jingwen, LI Huijun, GAO Qiuzhi |
| 图4 CR10-A0试样显微组织的TEM像、选区电子衍射(SAED)花样及EDS点扫描结果 |
| Fig.4 TEM image of the CR10-A0 sample (a), and EDS results and correponding selected area electron diffraction (SAED) patterns (insets) of δ-ferrite (b) and Laves (c) phases |
|