后续热处理对激光3D打印GH4099合金微观组织和高温力学性能的影响 |
| 赵亚楠, 郭乾应, 刘晨曦, 马宗青, 刘永长 |
|
Effects of Subsequent Heat Treatment on Microstructure and High-Temperature Mechanical Properties of Laser 3D Printed GH4099 Alloy |
| ZHAO Yanan, GUO Qianying, LIU Chenxi, MA Zongqing, LIU Yongchang |
| 图6 S1和S2热处理后LPBF制备GH4099合金样品的晶粒取向分布(GOS)图、晶粒GOS值统计图和晶界取向差分布图 |