选区激光熔化成形Al-Si-Fe-Mn-Ni合金的高温蠕变行为 |
| 韩英, 吴雨航, 赵春禄, 张靖实, 李振民, 冉旭 |
|
High-Temperature Creep Behavior of Selective Laser Melting Manufactured Al-Si-Fe-Mn-Ni Alloy |
| HAN Ying, WU Yuhang, ZHAO Chunlu, ZHANG Jingshi, LI Zhenmin, RAN Xu |
| 图8 SLM成形Al-Si-Fe-Mn-Ni合金在温度400 ℃、应力60 MPa条件下蠕变后断口附近的TEM像 |
| Fig.8 TEM images of the deformed microstructure near the fracture of SLMed Al-Si-Fe-Mn-Ni alloy after creeping under conditions of 400 oC and 60 MPa (White arrows represent dislocations, blue arrows represent Si phases, green arrows represent Al15(Fe, Mn, Ni)3Si2) (a) BF image (b) interaction behavior of IMCs and dispersed Si phases with dislocation and corresponding EDS results (c) high-magnification morphology of IMC and Si phase (d) SAED results of IMC and Si phase (e) HRTEM image of the dispersed Si phase |
|