Fe7(CoNiMn)80B13 共晶高熵合金的深过冷非平衡凝固行为及微观组织演变 |
| 王叶青, 付珂, 赵永柱, 苏礼季, 陈正 |
|
Non-Equilibrium Solidification Behavior and Microstructure Evolution of Undercooled Fe7(CoNiMn)80B13 Eutectic High-Entropy Alloy |
| WANG Yeqing, FU Ke, ZHAO Yongzhu, SU Liji, CHEN Zheng |
| 图5 ΔT = 57 K时Fe7(CoNiMn)80B13共晶高熵合金中共晶组织的EBSD分析 |
| Fig.5 EBSD analysis results of the eutectic structure in Fe7(CoNiMn)80B13 eutectic high-entropy alloys under ΔT = 57 K (a) phase map (b) EBSD map (Inset is the inverse pole figure (IPF) map of single α-(Fe, Co, Ni, Mn) phase) (c) pole figures of α-(Fe, Co, Ni, Mn) solid solution phase in crystal plane groups {100}, {110}, and {111}, respectively (Circles represent coincident orientations between M23B6 phase and α-(Fe, Co, Ni, Mn)) (d) pole figures of M23B6 phase in crystal plane groups {100}, {110}, and {111}, respectively |
|