Fe7(CoNiMn)80B13 共晶高熵合金的深过冷非平衡凝固行为及微观组织演变 |
| 王叶青, 付珂, 赵永柱, 苏礼季, 陈正 |
|
Non-Equilibrium Solidification Behavior and Microstructure Evolution of Undercooled Fe7(CoNiMn)80B13 Eutectic High-Entropy Alloy |
| WANG Yeqing, FU Ke, ZHAO Yongzhu, SU Liji, CHEN Zheng |
| 图3 ΔT = 23 K下Fe7(CoNiMn)80B13共晶高熵合金的SEM背散射电子(BSE)像及EDS线扫描图 |
| Fig.3 SEM back-scattered electron (BSE) images (a-d) and EDS line scanning result (e) of the Fe7(CoNiMn)80B13 eutectic high-entropy alloys with ΔT = 23 K (a, b) low (a) and high (b) magnifications, dendrites + fine structure (c) locally enlarged image of region 1 in Fig.3b, eutectic structure (d) locally enlarged image of region 2 in Fig.3b, net structure |
|