Al-Nb-B细化剂形核质点的弥散化及其对铸造铝合金组织及力学性能的影响 |
| 万杰, 李皓天, 刘书基, 路洪洲, 王立生, 张振栋, 刘春海, 贾建磊, 刘海峰, 陈豫增 |
|
Homogenization of Nuclei in Al-Nb-B Inoculant and Its Effect on Microstructure and Mechanical Properties of Cast Al Alloy |
| WAN Jie, LI Haotian, LIU Shuji, LU Hongzhou, WANG Lisheng, ZHANG Zhendong, LIU Chunhai, JIA Jianlei, LIU Haifeng, CHEN Yuzeng |
| 图7 经过不同状态熔融盐细化剂处理后静置不同时间铸态ZL104熔体的平均晶粒尺寸 |
| Fig.7 Average grain sizes of as-cast microstructure of ZL104 alloys treated with the molten salt-based inoculants in different states and maintained for different durations |
|