Al-Nb-B细化剂形核质点的弥散化及其对铸造铝合金组织及力学性能的影响 |
| 万杰, 李皓天, 刘书基, 路洪洲, 王立生, 张振栋, 刘春海, 贾建磊, 刘海峰, 陈豫增 |
|
Homogenization of Nuclei in Al-Nb-B Inoculant and Its Effect on Microstructure and Mechanical Properties of Cast Al Alloy |
| WAN Jie, LI Haotian, LIU Shuji, LU Hongzhou, WANG Lisheng, ZHANG Zhendong, LIU Chunhai, JIA Jianlei, LIU Haifeng, CHEN Yuzeng |
| 图5 不同状态熔融盐细化剂的SEM像 |
| Fig.5 SEM images of the molten salt-based inoculants in different states (a) as-cast (b) hot extruded at 280 oC with an extrusion ratio of 69 (c) cold rolled with a thickness reduction of 80% (CR-80%) (d) cold rolled with a thickness reduction of 90% (CR-90%) |
|