Al-Nb-B细化剂形核质点的弥散化及其对铸造铝合金组织及力学性能的影响 |
| 万杰, 李皓天, 刘书基, 路洪洲, 王立生, 张振栋, 刘春海, 贾建磊, 刘海峰, 陈豫增 |
|
Homogenization of Nuclei in Al-Nb-B Inoculant and Its Effect on Microstructure and Mechanical Properties of Cast Al Alloy |
| WAN Jie, LI Haotian, LIU Shuji, LU Hongzhou, WANG Lisheng, ZHANG Zhendong, LIU Chunhai, JIA Jianlei, LIU Haifeng, CHEN Yuzeng |
| 图4 铸态ZL104合金在添加熔炼和熔融盐细化剂前后微观组织的宏观照片和OM像 |
| Fig.4 OM images of as-cast ZL104 alloy under bright field (a-c) and polarization modes (d-f) (a, d) without inoculant (b, e) with smelting-based inoculant (c, f) with molten salt-based inoculant |
|