Fe-Cr合金气泡演化动力学的相场法模拟 |
| 刘彩艳, 冯泽华, 张云鹏, 余康, 吴璐, 马聪, 张静 |
|
Phase Field Simulation of Bubble Evolution Dynamics in Fe-Cr Alloys |
| LIU Caiyan, FENG Zehua, ZHANG Yunpeng, YU Kang, WU Lu, MA Cong, ZHANG Jing |
| 图7 位错应力场作用下Fe-0Cr和Fe-13Cr合金中气泡的演化 |
| Fig.7 Evolutions of bubbles under dislocation stress field in Fe-0Cr and Fe-13Cr alloys (a1-a5) Cg in Fe-0Cr alloy at 1200t0 (a1), 1500t0 (a2), 1950t0 (a3), 2250t0 (a4), and 3000t0 (a5), respectively (b1-b5) Cg in Fe-13Cr alloy at 1200t0 (b1), 1500t0 (b2), 1950t0 (b3), 2250t0 (b4), and 3000t0 (b5), respectively (c) area fraction of bubble under dislocation stress field (d) average radius of bubble under dislocation stress field |
|